Surface characterization of feldspathic ceramic using ATR FT-IR and ellipsometry after various silanization protocols
(Elsevier B.V., 2012-02-01)
Objectives. This study characterized the feldspathic ceramic surfaces after various silanization protocols.Methods. Ceramic bars (2 mm x 4 mm x 10 mm) (N = 18) of feldpathic ceramic (VM7, VITA Zahnfabrik) were manufactured ...
Can Heat Treatment Procedures of Pre-hydrolyzed Silane Replace Hydrofluoric Acid in the Adhesion of Resin Cement to Feldspathic Ceramic?
(Quintessence Publishing Co Inc, 2013-01-01)
Purpose: To evaluate the influence of heat treatment (HT) procedures of a pre-hydrolyzed silane on bond strength of resin cement to a feldspathic ceramic.Materials and Methods: Ceramic and composite blocks (N = 30) were ...
Can Heat Treatment Procedures of Pre-hydrolyzed Silane Replace Hydrofluoric Acid in the Adhesion of Resin Cement to Feldspathic Ceramic?
(Quintessence Publishing Co Inc, 2014)
Can Heat Treatment Procedures of Pre-hydrolyzed Silane Replace Hydrofluoric Acid in the Adhesion of Resin Cement to Feldspathic Ceramic?
(Quintessence Publishing Co Inc, 2014)
Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions
(Elsevier B.V., 2007-11-01)
Objectives. This study evaluated the durability of bond strength between resin cement and a feldspathic ceramic submitted to different etching regimens with and without silane coupling agent application.Methods. Thirty-two ...
Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions
(Elsevier B.V., 2007-11-01)
Objectives. This study evaluated the durability of bond strength between resin cement and a feldspathic ceramic submitted to different etching regimens with and without silane coupling agent application.Methods. Thirty-two ...